custom cover glass,dragontrail glass,gorilla glass
Technical data
Aluminosilicate glass |
Soda lime glass |
|||||
Type |
corning gorilla glass |
dragontrail glass |
Schott Xensat |
panda glass |
NEG T2X-1 glass |
float glass |
Thickness |
0.4mm,0.5mm,0.55mm,0.7mm 1mm,1.1mm,1.5mm,2mm |
0.55mm,0.7mm,0.8mm 1.0mm,1.1mm,2.0mm |
0.55mm,0.7mm 1.1mm |
0.7mm,1.1mm |
0.55mm,0.7mm 1.1mm |
0.55mm,0.7mm,1.1mm,2mm 3mm,4mm,5mm,6mm |
Chemical strengthened |
DOL≥ 40um CS≥700Mpa |
DOL≥ 35um CS≥650Mpa |
DOL≥ 35um CS≥650Mpa |
DOL≥ 32um CS≥600Mpa |
DOL≥ 35um CS≥650Mpa |
DOL≥ 8um CS≥450Mpa |
Hardness |
≥9H |
≥9H |
≥7H |
≥7H |
≥7H |
≥7H |
Transmittance |
>92% |
>90% |
>90% |
>90% |
>90% |
>89% |
Surface treatment: Anti glare coating,anti reflective coating,anti fingerprint,ito conductive coating available.
Tempered option: Thermally tempered,heat strengthened,chemically strengthened(chemically tempered).
Processing
Cover Glass Type
1. Aluminosilicate glass refers to the glass with silica and alumina as the main components, in which the alumina content can reach more than 20%. The coordination number of the aluminum ion depends on the R2O (alkali metal oxide) content.
Gorilla Glass produced by Corning is one kinf of aluminosilicate glass.because of this superior performance in.
Superior scratch resistant good chemical stability,
electrical insulation
mechanical strength
low thermal expansion coefficient
high temperature viscosity.
High price
It is widely used on high-class touch screen and phone,or other portable devices.
Soda-lime glass, most common form of glass produced, it is inexpensive, chemically stable, reasonably hard, and extremely workable glass,it is enough for basic requirement,those make it most popular and widely use on touch panel in various application.
Annealed glass VS heat strengthened glassVS thermally tempered glass.
What is the difference between thermally tempered and chemically strengthened glass.